Tungsten oxide nanowire may be prepared by hydrothermal method using Na2WO4•2H2O and HCl as raw materials with Na2SO4 as additive. Hydrothermal Method to Prepare Tungsten Trioxide Nanowire 1. Weigh 3.68g (0.011mol) Na2WO4•2H2O into 20ml deionized water and stir it to dissolve; 2. Add 3M HCl to the above solution dropwise, stir it until the white precipitate no longer generated, and adjust the pH≈1; 3. Add in certain amount of 0.5M Na2SO4, continue to stir for 2h and transfer the solution…