How to Prepare High-purity Ammonium Paratungstate?

How to prepare high-purity ammonium paratungstate? The researchers proposed a method for preparing high-purity APT. This method improves the quality of ammonium paratungstate and reduces the production cost of high-purity APT.

More details, please visit:
http://ammonium-paratungstate.com/index.html

how to prepare high-purity ammonium paratungstate image

A Preparation Method of High-purity Ammonium Paratungstate
Step One: Put APT into the feed bin and send it into the rotary furnace through the screw feeder at a constant speed. Control the calcination temperature and atmosphere in the rotary furnace. The feed volume is 150 kg/h. The calcination temperature is 550 °C in the first zone, 640 °C in the second zone, and 680 °C in the third zone, respectively. After calcining, the conversion rate of APT to tungsten trioxide reached 98.85%.
Step Two: Control the temperature of the 150 g/L ammonia solution at 95 °C, and the liquid-solid ratio at 3:1 ml/g. Tungsten trioxide is added into the solution while stirring, and reacted for 1.5h to obtain an ammonium tungstate solution, and then filtered.
Step Three: After filtering the ammonium tungstate solution, measure it into an evaporative crystallization pot for evaporative crystallization, control the evaporative crystallization steam at 1-4 kgf/cm2, when the specific gravity of the solution is close to 1.05 g/cm3, stop heating, and separate the crystal and mother liquor to obtain aqueous ammonium paratungstate.
Step Four: Remove excess water in aqueous ammonium paratungstate by steam drying to obtain high purity ammonium paratungstate.

Comments are closed.

Address: 3F, No.25-1 WH Rd., Xiamen Software Park Ⅱ, FJ 361008,China Copyright © 1997 - 2024 CTIA All Rights Reserved
Phone:+86-592-5129696,+86-592-5129595;    Email: sales@chinatungsten.com
旧版
Baidu
map